In718 Nickel-based Superalloy powder Spherical Nickel-based 3D printed powder

Short Description:

Granularity: 15-53um, 53-150um customized

Purity: Custom

Product morphology: dark grey amorphous powder;

Product features: high purity, complete specifications, controllable granularity, stable quality; Granularity range: specific according to customer requirements for production;


Product Detail

Product Tags

Product introduction:

In718 powder is a super alloy powder material produced by powder metallurgy process. It is composed of cobalt, chromium, iron, molybdenum, aluminum, titanium and nickel. In718 powder has high strength at high temperature and good corrosion resistance, which is widely used in aerospace and petrochemical fields. The preparation process of In718 powder is generally gas atomization or water atomization, and the required shape parts can be obtained by pressing and sintering after preparation and forming. This powder material has excellent comprehensive properties, including high strength, excellent corrosion resistance, good fatigue life and high stiffness at high temperature, so it has important application value in high temperature, high pressure, strong corrosion environment.

Product application:

In718 powder has a wide range of applications in aerospace, military, nuclear energy, Marine and petrochemical fields, it can manufacture a variety of high-strength structural parts, engine parts, valves, turbine blades, forging dies, heat-resistant strengthening devices and complex pipelines, valves, etc

Product nature:

1. High strength: In718 powder has high yield strength and tensile strength, as well as excellent toughness. Its strength decreases with the increase of temperature, but it can still maintain a certain strength at high temperature.
2. Good corrosion resistance: In718 powder has good corrosion resistance to most acids, salts and water vapor, with the performance of use in high temperature and high pressure environment.
3. High temperature oxidation resistance: In718 powder has good high temperature oxidation resistance and can maintain good corrosion resistance at high temperature. This makes it suitable for parts used at high temperatures, such as engine jets, turbine blades, etc.
4. Good processability: In718 powder can be made into parts of different shapes by metal injection molding, hot static pressing powder and other processes.
5. Excellent fatigue life: In718 powder has good fatigue life and toughness in long-term use, which can meet the requirements of high-performance structural components.

Product name Precipitation Strengthened Nickel-Based Superalloys(IN718)
Material Ni Cr B Si Fe etc.
Certification ISO9001
Place of origin Deyang,China
price 1-5kg :sample price over 5kg: bulk price
our service Product customization, order tracking, double quality inspection, factory report.
Size 10-45 um
15-53 um
45-105 um
53-150 um
oxygen content ≤200ppm
Apparent Density 15-53μm (VIGA):≥4.30g/cm3
Tap density 15-53μm (VIGA):≥4.50g/cm3
650 ℃ high temperature performance tensile strength:1250±50MPa
yield strength:1090±50MPa
Elongation:13%
Sample Availiable
Application 3D printing,thermal spray,additive manufacturing etc.

Quality certificate: